蜂窝活性炭聚合氯化铝工厂价格
更新时间:2025-04-14 18:47:31 浏览次数:40 公司名称: 普邦环保材料有限公司
产品参数 | |
---|---|
产品价格 | 电议 |
发货期限 | 电议 |
供货总量 | 电议 |
运费说明 | 电议 |
规格 | 100*100*100mm、100*100*50mm、100*100*200mm |
品牌 | 中航 |
产地 | 北京 |
碘值 | 500 |


The two is to look at the honeycomb activated carbon products produced by the bubble, if the bubble is more the better the quality of the product. We can do a little experiment, a handful of honeycomb activated carbon products into the water, because the water penetration effect, water will be immersed in the pores of activated carbon, so the pore in the air, resulting in a series of very small bubbles, pulled out a tiny bubbles lines in the water, at the same time also issued Zizi bubble sound, looked very interesting. If this phenomenon is very serious, and the longer the duration, then it is proved that the honeycomb activated carbon product pore structure is very developed, that is, the better adsorption performance of honeycomb activated carbon.
普邦环保材料有限公司企业主要产品有 四川阿坝聚合氯化铝等产品。普邦环保材料有限公司的开发紧追时代潮流,不断推出更新颖、更优质的普邦环保材料有限公司系列产品。
十年前全球都是采用煤质柱状活性炭来净化废气,由于柱状活性炭在废气处理塔中堆放过多,会倒至风阻过大,废气无法从活性炭中经过,所以无法达到净化的作用,如堆放过少,那么净化效果就无法达到 排放标准。 前几年蜂窝状活性炭的诞生从此推向净化行业的另一个新阶段。
3、蜂窝状活性炭特点
蜂窝状活性炭的特点就是净化效果好,风速阻力小,完全可以达到 废气排放标准。
zhyh
蜂窝活性炭生产方法 步是:褐煤或烟煤与焦煤分别破碎到小于2毫米(mm),然后按质量比褐煤或烟煤∶焦煤为1∶0.2—0.5混合后,再研磨至74米(μm)以下,会得到混合均匀的煤粉。
蜂窝活性炭生产方法第二步是:1、沥青含量大于等于55%高温煤焦油预热至120—150℃;2、乳化剂水溶液的配制,在水中加入高温煤焦油质量的2—6%表面活性剂和高温煤焦油质量的0.5—2%的稳定剂,并预热至80—90摄氏度(℃)形成乳化剂水溶液,3、按质量比为高温煤焦油∶乳化剂水溶液=1∶0.3—0.7,在搅拌条件下,将高温煤焦油加入乳化剂水溶液中制成乳化煤焦油。
蜂窝活性炭生产方法第三步是:按质量比为煤粉∶乳化煤焦油∶水∶水溶性粘合剂∶润滑剂=34—57∶30—36∶6—29∶3—5∶2—3,将其加入捏合机当中搅拌均匀后,能够制成可塑性的煤泥。
蜂窝活性炭生产方法第四步是:可塑性煤泥经过真空练泥机或挤出成型机处理,使得煤泥混合均匀,然后在成型机中用60—100目的丝网中过滤除掉大颗粒物质。
蜂窝活性炭生产方法第五步:练泥处理后的煤泥加入装有蜂窝钢模具的挤出成型机中,进行成型,得到湿的蜂窝体。
蜂窝活性炭生产方法第六步:湿的蜂窝体干燥至水分低于2%;以惰性气体作为保护气,按升温速度3-5℃/min(摄氏度/分钟)加热到600—800℃,并且在此温度下炭化2—3个小时;然后按升温速度5—15℃/min(摄氏度/分钟)升温到750—850℃,用水蒸气活化3—15个小时,经过多道工艺终于制成蜂窝活性炭。